What caused my layered glass pieces to look so flat?

By HotPot Norge, Jan 26 2013 10:00AM

If the glass piece has flattened out too much, the piece is over fired.


To prevent this from happening, reduce the firing time.


During the firing process, lift the lid of the microwave kiln to see how far the fusing process is.

If the desired results have not been achieved, continue firing in 20-30 seconds intervals.

Repeat this till you have your piece fused to the level you want.